Calculator:

Gypsonit (for machine use)
  • Mineral
  • Thermal insulated
  • Sound insulated
  • Eco friendly and safe
Composition
Gypsum, polymer additives.
Recommended use
Designed for interior works, can be applied on natural stone (tuff), concrete, cement-sand, bricks, concrete blocks and drywall surfaces.
Surface preparation
  • Prior to application  remove dirt, dust, oil, paint, etc. from the surface .
  • It is recommended to treat the surface with “SHEN” beton contact before the works.
  • The plaster can be applied after 4-5 hours.

Making the mixture

  • Pour 18.2-19.6l of water per 35kg of dry mixture into a clean container .
  • Gradually add dry mixture and stir with a mixer to obtain paste-like mass without lumps.
Application
  • Apply the mixture with a stainless metallic putty knife or spatula on the surface.
  • It is recommended to work at air temperatures not lower than +10°C and relative humidity of not more than 75%.
  • When the work is over or suspended, carefully wash the tools.
  • Dispose of the paper bags and mixture leftovers as prescribed by local legislation.
  • For fast plaster drying expose to air and moderate ventilation.

 

Temperature of the base when applying

from +10°C to +30°C

Amount of water per 1kg of dry mixture

520-560ml

Amount of water per 35kg of dry mixture

18.2-19.6l

Recommended thickness of layer

not less than 1cm

Time of serviceability of the mixture

 

not less than 30 minutes

Shrinkage

not more than 0.8mm/m

 

Dry mixture consumption per 1cm thick layer More precisely, the consumption depends on the surface quality and thickness of plaster layer.

11kg/1m²

 

35kg/3.18m²

 

Sizes available

Polypropylene bags. Net weight 35 kg. 

Storage
Store in undamaged packaging, on palettes, in dry premises, at temperatures under 45°С and humidity under 75%, for 3 months after the manufacturing date indicated on the package.
Terms of use
  • Store in a place inaccessible to children.
  • When working, protect respiratory organs.
  • Avoid contact with skin.
  • In case of eye contact, rinse with clean water and, if needed, apply to doctor.
Attention
  • It is prohibited to add water into the mixture after its tightening (beginning of setting): this can cause decreased mixture adhesion and cracking.
  • When working in conditions other than normal, the performances may deviate from the ones indicated in the table.